Titre: | The thermal and thermomechanical behaviors of Spartium junceum flour reinforced polypropylene composites: effects of treatment and flour content |
Auteur(s): | Nouar, Y Nekkaa, S Fernández-García, M López, D |
Mots-clés: | Composites polypropylene spartium junceum alkali treatment silane coupling agent thermal stability interfacial adhesion |
Date de publication: | 16-jan-2019 |
Collection/Numéro: | Composite Interfaces;25(3):1-23 · April 2018 |
Résumé: | The effects of Spartium junceum(SJ) flour content, treatment time on the
thermal and thermomechanical properties of polypropylene/Spartium
junceumflour (PP/SJ) composites were studied. In order to improve
the interfacial adhesion between the PP matrix and the SJ flour, SJ
flour was treated with NaOH (2 wt%) for 8, 24 and 48 h at ambient
temperature, respectively, and treated by vinyltrimethoxysilane
(VTMS) (5 wt%). The results of thermogravimetric analysis (TGA) of
SJ flour shows that the treatment improves the thermal stability of
SJ flour. DSC analysis measurements illustrates that the addition of SJ
flour increase the degree of crystallinity X
c
, which indicate that the SJ
flour plays a significant role in heterogeneous nucleating of PP matrix.
The chemical treatments significantly affect the storage modulus of
composite, where E′increases for composites with treated flour in
comparison to the untreated ones. |
URI/URL: | http://dspace.univ-setif.dz:8888/jspui/handle/123456789/3066 |
ISSN: | 0927-6440 (Print) 1568-5543 (Online) |
Collection(s) : | Articles
|
Fichier(s) constituant ce document :
|
Tous les documents dans DSpace sont protégés par copyright, avec tous droits réservés.
|